Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 172 MPa @Temperature 150 °C |
24900 psi @Temperature 302 °F |
ISO 604 |
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex.. |