Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 172 MPa @Temperature 260 °C |
25000 psi @Temperature 500 °F |
Dry, Autoclave with Post-Cure; ASTM D695 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Compressive Strength | 172 MPa @Temperature 150 °C |
24900 psi @Temperature 302 °F |
ISO 604 |
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex.. |