Polymer Property : Compressive Strength = 3.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 3.00 - 7.00 MPa

@Temperature 100 °C
435 - 1020 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable
Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va..
Compressive Strength 3.00 - 7.00 MPa

@Temperature 1260 °C
435 - 1020 psi

@Temperature 2300 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable
Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari..
Compressive Strength 3.00 MPa

@Temperature 200 °C
435 psi

@Temperature 392 °F
Elisto THERMOSTAR® XPS Mold Insulation Material
Lateral insulationInformation provided by elisto