Material Notes:
Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
After drying at 110°C
Particle Size <= 7000 µm
<= 7000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 1.00 - 5.00 MPa

@Temperature 1260 °C
145 - 725 psi

@Temperature 2300 °F
Cold Crushing Strength
3.00 - 7.00 MPa

@Temperature 100 °C
435 - 1020 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.190 - 0.290 W/m-K

@Temperature 100 °C
1.32 - 2.01 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.190 - 0.290 W/m-K

@Temperature 600 °C
1.32 - 2.01 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.270 - 0.370 W/m-K

@Temperature 1260 °C
1.87 - 2.57 BTU-in/hr-ft²-°F

@Temperature 2300 °F
Maximum Service Temperature, Air 1350 °C
2460 °F
Shrinkage -1.50 - 1.50 %

@Temperature 1260 °C
-1.50 - 1.50 %

@Temperature 2300 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 42 %
42 %
SiO2 40 %
40 %
Descriptive Properties Value Comments
ASTM Classification Q
Material Consumption per 1 m3 1000 kg
Mixing Water 30-35 liters
per 100 kgs dry material