Mechanical Properties Metric English Comments
Compressive Strength 3.50 - 4.50 MPa

@Temperature 100 °C
508 - 653 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable
Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re..
Compressive Strength 3.50 - 4.50 MPa

@Temperature 100 °C
508 - 653 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE LW Refractory Insulating Castable
Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also ava..
Compressive Strength 3.50 - 4.50 MPa

@Temperature 100 °C
508 - 653 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable
Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod..
Compressive Strength 3.50 - 4.50 MPa

@Temperature 1200 °C
508 - 653 psi

@Temperature 2190 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable
Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod..