Material Notes:
Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.05 - 1.15 g/cc
0.0379 - 0.0415 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 3.50 - 4.50 MPa

@Temperature 100 °C
508 - 653 psi

@Temperature 212 °F
Cold Crushing Strength
3.50 - 4.50 MPa

@Temperature 1200 °C
508 - 653 psi

@Temperature 2190 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.190 - 0.290 W/m-K

@Temperature 100 °C
1.32 - 2.01 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.220 - 0.320 W/m-K

@Temperature 600 °C
1.53 - 2.22 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.290 - 0.390 W/m-K

@Temperature 1200 °C
2.01 - 2.71 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Shrinkage -1.20 - 0.800 %

@Temperature 1200 °C
-1.20 - 0.800 %

@Temperature 2190 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 29 %
29 %
SiO2 32 %
32 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 1025 kg
Mixing Water 34-38 liters
per 100 kgs dry material
Users viewing this material also viewed the following: