Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 400 MPa @Temperature 21.1 °C |
58000 psi @Temperature 70.0 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 400 MPa @Temperature 21.1 °C |
58000 psi @Temperature 70.0 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 400 MPa @Temperature 23.9 °C |
58000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:.. |
|||
Compressive Strength | 400 MPa @Temperature 149 °C |
58000 psi @Temperature 300 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4503 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Compressive Strength | 400 MPa @Temperature 23.9 °C |
58000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Compressive Strength | 400 MPa @Temperature 23.0 °C |
58000 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® HD 800 Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Compressive Strength | 400 MPa @Temperature 23.0 °C |
58000 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® LC 400 GL Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |