Polymer Property : Compressive Strength = 44.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 44.0 MPa

@Strain 2 %
6380 psi

@Strain 2 %
ISO 604
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data)
Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit..
Compressive Strength 44.0 MPa

@Strain 2 %
6380 psi

@Strain 2 %
ISO 604
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data)
Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c..
Compressive Strength 44.0 MPa

@Strain 1 %
6380 psi

@Strain 1 %
ISO 604
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data)
Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l..
Compressive Strength 44.0 MPa

@Strain 1 %
6380 psi

@Strain 1 %
ISO 604
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data)
This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap..