Mechanical Properties Metric English Comments
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data)
Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal fo..
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data)
Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, ..
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data)
This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin..
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data)
This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie..
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data)
Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX..
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data)
This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu..
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data)
Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr..
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data)
Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou..
Compressive Strength 31.0 MPa

@Temperature 110 °C
4500 psi

@Temperature 230 °F
Pyrotek Pyrocast PT-190 Refractory Cast Parts
Pyrocast PT-190 is an extremely dense alumina based refractory. It is best suited for applications where high velocity metal erosion potential is a problem, due to its strength and abrasion resista..
Compressive Strength 31.0 MPa

@Temperature 149 °C
4500 psi

@Temperature 300 °F
ASTM D 695
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material
Meldin 1357 offers the lowest wear rate and coefficient of friction, which makes it the best candidate for tribological applications. In addition, its self-lubricating properties allow it to operat..