Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00220 GPa @Strain 20 % |
0.319 ksi @Strain 20 % |
ISO-7743 |
Vicone High Performance Rubber VicoSilâ„¢ 139DLK-BL High Performance Silicone Rubber FDA Approved |