Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 18.6 GPa @Temperature 71.1 °C |
2700 ksi @Temperature 160 °F |
Dry; Autoclave, 50 psi, 90min; ASTM D695 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Compressive Modulus | 18.6 GPa @Temperature 93.0 °C |
2700 ksi @Temperature 199 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric Information provided by HexCel |