Mechanical Properties Metric English Comments
Compressive Modulus 18.6 GPa

@Temperature 71.1 °C
2700 ksi

@Temperature 160 °F
Dry; Autoclave, 50 psi, 90min; ASTM D695
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring ..
Compressive Modulus 18.6 GPa

@Temperature 93.0 °C
2700 ksi

@Temperature 199 °F
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric
Information provided by HexCel