Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00345 GPa | 0.500 ksi | Dry Modulus of Rupture, 50% clay/50% flint, cast bars |
Old Hickory M-23 Tennessee Ball Clay This is a very high quality porcelain grade ball clay. It has fine particle size distribution for excellent plasticity and strength in pressing or plastic forming application. the low Fe2O3 and TiO2.. |
|||
Modulus of Rupture | 0.00345 GPa | 0.500 ksi | Dry Modulus of Rupture, 50% clay/50% flint, cast bars |
Old Hickory MCB-11 Tennessee Ball Clay A clay with excellent kaolin content and virtually no carbon content. It is highly plastic with excellent fired brightness and is an excellent clay for a variety of ceramic glaze and porcelain compo.. |
|||
Modulus of Rupture | 0.00345 GPa | 0.500 ksi | Dry Modulus of Rupture, 50% clay/50% flint, cast bars |
Old Hickory S-4 Tennessee Ball Clay The S-4 clay is designed for all types of casting formulas ranging from low fire earthenware to vitreous compositions. It has excellent response to deflocculation and very good casting rate while ma.. |
|||
Modulus of Rupture | 0.00345 GPa | 0.500 ksi | dry |
Imerys Kingsley - Rogersâ„¢ Kaolin Information provided by Imerys |
|||
Modulus of Rupture | 0.00345 GPa | 0.500 ksi | |
Zircar Refractory Composites RS-A Refractory Sheet ZRCI`s Refractory Sheet Type RS-A Moldable is a tough ceramic fiber reinforced insulation which contains no asbestos. Developed as an asbestos board replacement for induction coil liners and molten .. |