Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00539 - 0.00686 GPa @Temperature 1400 °C |
0.782 - 0.995 ksi @Temperature 2550 °F |
|
Chosun Refractories CRAG-L38 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |