Mechanical Properties Metric English Comments
Modulus of Rupture 0.004905 - 0.006867 GPa

@Temperature 1400 °C
0.7114 - 0.9960 ksi

@Temperature 2550 °F
Chosun Refractories CRZG-L30 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.005886 - 0.006867 GPa

@Temperature 1400 °C
0.8537 - 0.9960 ksi

@Temperature 2550 °F
Chosun Refractories CRAG-L42 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).