Chosun Refractories CRZG-L30 Shroud Nozzle

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CRZG-L30 Shroud Nozzle.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.20 g/cc
0.116 lb/in³
Porosity 16 %
16 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.004905 - 0.006867 GPa

@Temperature 1400 °C
0.7114 - 0.9960 ksi

@Temperature 2550 °F
Compressive Strength 22.6 MPa
3270 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 6.33 µm/m-°C

@Temperature 1000 °C
3.52 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
ZrO2 69 %
69 %
Descriptive Properties Value Comments
Chemical Analysis (%), FC+SiC 26+0
Remarks Corrosion resistance for slag