Mechanical Properties Metric English Comments
Modulus of Rupture 0.0207 GPa

@Temperature 1010 °C,
Time 86400 sec
3.00 ksi

@Temperature 1850 °F,
Time 24.0 hour
Zircar Refractory Composites RS-200 Refractory Sheet
ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Modulus of Rupture 0.0207 GPa

@Temperature 1010 °C,
Time 86400 sec
3.00 ksi

@Temperature 1850 °F,
Time 24.0 hour
Zircar Refractory Composites RS-201 Refractory Sheet
ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Modulus of Rupture 0.0207 GPa

@Temperature 1010 °C,
Time 86400 sec
3.00 ksi

@Temperature 1850 °F,
Time 24.0 hour
Zircar Refractory Composites RS-202 Refractory Sheet
ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Modulus of Rupture 0.0207 GPa
3.00 ksi
BNZ Materials CS85 High Temperature Structural Insulation
NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,..
Modulus of Rupture 0.0207 GPa
3.00 ksi
BNZ Materials Transite 1000 Low Temperature Industrial Board
These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind..
Copyright © lookpolymers.com All Rights Reserved