Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0207 GPa @Temperature 1010 °C, Time 86400 sec |
3.00 ksi @Temperature 1850 °F, Time 24.0 hour |
|
Zircar Refractory Composites RS-200 Refractory Sheet ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Modulus of Rupture | 0.0207 GPa @Temperature 1010 °C, Time 86400 sec |
3.00 ksi @Temperature 1850 °F, Time 24.0 hour |
|
Zircar Refractory Composites RS-201 Refractory Sheet ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Modulus of Rupture | 0.0207 GPa @Temperature 1010 °C, Time 86400 sec |
3.00 ksi @Temperature 1850 °F, Time 24.0 hour |
|
Zircar Refractory Composites RS-202 Refractory Sheet ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Modulus of Rupture | 0.0207 GPa | 3.00 ksi | |
BNZ Materials CS85 High Temperature Structural Insulation NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,.. |
|||
Modulus of Rupture | 0.0207 GPa | 3.00 ksi | |
BNZ Materials Transite 1000 Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |