Mechanical Properties Metric English Comments
Modulus of Rupture 0.0310 GPa

@Temperature 510 °C,
Time 86400 sec
4.50 ksi

@Temperature 950 °F,
Time 24.0 hour
Zircar Refractory Composites RS-200 Refractory Sheet
ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Modulus of Rupture 0.0310 GPa
4.50 ksi
parallel to thickness
Zircar Refractory Composites RS-1200 Refractory Sheet
ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12..
Modulus of Rupture 0.0310 GPa

@Temperature 510 °C,
Time 86400 sec
4.50 ksi

@Temperature 950 °F,
Time 24.0 hour
Zircar Refractory Composites RS-201 Refractory Sheet
ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Modulus of Rupture 0.0310 GPa

@Temperature 510 °C,
Time 86400 sec
4.50 ksi

@Temperature 950 °F,
Time 24.0 hour
Zircar Refractory Composites RS-202 Refractory Sheet
ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Copyright © lookpolymers.com All Rights Reserved