Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0310 GPa @Temperature 510 °C, Time 86400 sec |
4.50 ksi @Temperature 950 °F, Time 24.0 hour |
|
Zircar Refractory Composites RS-200 Refractory Sheet ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Modulus of Rupture | 0.0310 GPa | 4.50 ksi | parallel to thickness |
Zircar Refractory Composites RS-1200 Refractory Sheet ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12.. |
|||
Modulus of Rupture | 0.0310 GPa @Temperature 510 °C, Time 86400 sec |
4.50 ksi @Temperature 950 °F, Time 24.0 hour |
|
Zircar Refractory Composites RS-201 Refractory Sheet ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Modulus of Rupture | 0.0310 GPa @Temperature 510 °C, Time 86400 sec |
4.50 ksi @Temperature 950 °F, Time 24.0 hour |
|
Zircar Refractory Composites RS-202 Refractory Sheet ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |