Mechanical Properties Metric English Comments
Modulus of Rupture 0.000660 GPa
0.0957 ksi
Pyrotek Pyrotherm TF-19 Lightweight, non-RCF insulation board for ovens, furnaces, kilns and vessels
Pyrotherm TF-19 is a high-temperature board providing high strength and excellent workability. It is composed of mineral fiber and selected mineral additives.ApplicationsPot cradle insulation (for ..
Modulus of Rupture 0.000660 GPa
0.0957 ksi
As Received, Parallel to thickness
Zircar Ceramics ECO-1200A Alumina-Silica Insulation
This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-1200 is part of hundreds of different thermal process systems. Information provid..