Polymer Property : Modulus of Rupture = 0.812 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00560 GPa
0.812 ksi
parallel to thickness
Zircar Refractory Composites ZIRCAL-45 Refractory Board
Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com..