Zircar Refractory Composites ZIRCAL-45 Refractory Board

Category Ceramic
Manufacturer Zircar Refractory Composites, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Refractory Composites ZIRCAL-45 Refractory Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength combined with high thermal insulating value make it ideal for many fireproofing and heat processing equipment applications up to 650°C(1202oF). ZIRCAL-45 is highly damage resistant, non-corroding, and extremely water-resistant.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 0.760 g/cc
0.0275 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00560 GPa
0.812 ksi
parallel to thickness
Compressive Yield Strength 70.0 MPa
10200 psi
at 5% deformation, parallel to thickness
Thermal Properties Metric English Comments
CTE, linear 3.10 µm/m-°C

@Temperature 20.0 - 700 °C
1.72 µin/in-°F

@Temperature 68.0 - 1290 °F
5.50 µm/m-°C

@Temperature 20.0 °C
3.06 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.120 W/m-K

@Temperature 200 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 392 °F
parallel to thickness
0.120 W/m-K

@Temperature 400 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 752 °F
parallel to thickness
0.120 W/m-K

@Temperature 600 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1110 °F
parallel to thickness
Maximum Service Temperature, Air 650 °C
1200 °F
Shrinkage 0.400 %

@Temperature 650 °C,
Time 43200 sec
0.400 %

@Temperature 1200 °F,
Time 12.0 hour
Linear reheat (perpendicular to thickness)
Component Elements Properties Metric English Comments
Other <= 5.0 %
<= 5.0 %
Electrical Properties Metric English Comments
Volume Resistivity 9.80e+7 ohm-cm
9.80e+7 ohm-cm
ASTM D257
Dielectric Strength 1.77 kV/mm
45.0 kV/in
ASTM D495
Processing Properties Metric English Comments
Moisture Content 3.0 %
3.0 %
Descriptive Properties Value Comments
CaSiO3, % 95