Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 130 kJ/m² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 3441R PC (Europe-Africa-Middle East) Lexan 3441R is a medium viscosity, 10% glass reinforced polycarbonate grade, compliant with European food contact regulation EC Directive 2002/72/EC. The grade is especially designed for application.. |
|||
Izod Impact, Unnotched (ISO) | 130 kJ/m² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
DuPont Performance Polymers Crastin® FG6129 NC010 PBT
(Unverified Data**) Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part.. |
|||
Izod Impact, Unnotched (ISO) | 130 kJ/m² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |