Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 61.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 130 kJ/m²

@Temperature -30.0 °C
61.9 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® 3441R PC (Europe-Africa-Middle East)
Lexan 3441R is a medium viscosity, 10% glass reinforced polycarbonate grade, compliant with European food contact regulation EC Directive 2002/72/EC. The grade is especially designed for application..
Izod Impact, Unnotched (ISO) 130 kJ/m²

@Temperature -30.0 °C
61.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
DuPont Performance Polymers Crastin® FG6129 NC010 PBT  (Unverified Data**)
Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part..
Izod Impact, Unnotched (ISO) 130 kJ/m²

@Temperature 23.0 °C
61.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..