Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 200 kJ/m² @Temperature -20.0 °C |
95.2 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1U |
Borealis Daplen™ EE065AI Polypropylene Elastomer Modified Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu.. |