Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 180-1U |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced PA 6-Copolymer, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
conditioned; ISO 180-1U |
Lanxess Durethan® BKV 15 H.3 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® V9280LW PET (Europe-Africa-Middle East) 40% Glassfiber / Mineral Filled PET, Impact Modifier, Mold Release, Heat StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East) VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecopet® PT74 GR30 BK002 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
conditioned; ISO 180-1U |
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPC345G30 Polypropylene Copolymer, 30% Glass Filled SAXALEN PPC345G30 is a 30% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Sax Polymers SAXATEC 4115 Acrylonitrile Styrene Acrylate SAXATEC 4115 is a medium viscosity, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX .. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Sax Polymers SAXATEC 4120 Acrylonitrile Styrene Acrylate SAXATEC 4120 is a easy lowing, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym.. |