Tensile Strength 150 MPa

@Temperature 70.0 °C,
Time 180000 sec
21800 psi

@Temperature 158 °F,
Time 50.0 hour
62% RH
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
Tensile Strength 150 MPa

@Temperature 23.0 °C
21800 psi

@Temperature 73.4 °F
ISO 527
BASF Ultradur S 4090 G6 30% Glass Filled PBT
Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati..