Polymer Property : Tensile Strength = 260 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 260 MPa

@Thickness 8.00 - 25.0 mm
>= 37700 psi

@Thickness 0.315 - 0.984 in
Temper T651
Constellium DOKIMA® Rolled Plate Aluminum
DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct..
Tensile Strength >= 260 MPa

@Thickness 25.0 - 60.0 mm
>= 37700 psi

@Thickness 0.984 - 2.36 in
Temper T651
Constellium DOKIMA® Rolled Plate Aluminum
DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct..
Tensile Strength >= 260 MPa

@Thickness 60.0 - 150 mm
>= 37700 psi

@Thickness 2.36 - 5.91 in
Temper T651
Constellium DOKIMA® Rolled Plate Aluminum
DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct..
Tensile Strength >= 260 MPa

@Thickness 80.0 - 120 mm
>= 37700 psi

@Thickness 3.15 - 4.72 in
Temper H111; Standard EN 485-2
Constellium PLAN 5083 Aluminum Rolled Plate
Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m..
Tensile Strength >= 260 MPa

@Thickness 80.0 - 100 mm
>= 37700 psi

@Thickness 3.15 - 3.94 in
Tempers O/H111; Standard EN 485-2
Constellium Planoxal® 50 Aluminum plate
Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main..
Tensile Strength >= 260 MPa

@Thickness 80.0 - 120 mm
>= 37700 psi

@Thickness 3.15 - 4.72 in
Temper H111; Standard EN 485-2
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug..