Polymer Property : Tensile Strength = 315 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 315 MPa

@Diameter 20.0 - 40.0 mm
45700 psi

@Diameter 0.787 - 1.57 in
United Cast Bar Unibar 350 Continuously Cast Iron
Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a..