Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

United Cast Bar Unibar 350 Continuously Cast Iron

Category Metal , Ferrous Metal , Cast Iron , Gray Cast Iron
Manufacturer United Cast Bar
Trade Name Unibar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF United Cast Bar Unibar 350 Continuously Cast Iron.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a good surface finish. Noise and vibration damping are good in this grade.Unibar-350 can be hardened by conventional methods, to Rc 50 on the bar surface.Information provided by United Cast Bar Ltd.
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 230 - 300

@Load 3000 kg
230 - 300

@Load 6610 lb
10 mm ball
Tensile Strength 225 MPa

@Diameter 150 - 300 mm
32600 psi

@Diameter 5.91 - 11.8 in
250 MPa

@Diameter 80.0 - 150 mm
36300 psi

@Diameter 3.15 - 5.91 in
280 MPa

@Diameter 40.0 - 80.0 mm
40600 psi

@Diameter 1.57 - 3.15 in
315 MPa

@Diameter 20.0 - 40.0 mm
45700 psi

@Diameter 0.787 - 1.57 in
Component Elements Properties Metric English Comments
Carbon, C 2.95 - 3.45 %
2.95 - 3.45 %
Iron, Fe 92.58 - 94.21 %
92.58 - 94.21 %
as balance
Manganese, Mn 0.60 - 0.80 %
0.60 - 0.80 %
Phosphorous, P 0.10 - 0.20 %
0.10 - 0.20 %
Silicon, Si 2.1 - 2.9 %
2.1 - 2.9 %
Sulfur, S 0.040 - 0.070 %
0.040 - 0.070 %
Copyright © lookpolymers.com All Rights Reserved