Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 517 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 517 MPa

@Thickness 25.4 - 38.1 mm
>= 75000 psi

@Thickness 1.00 - 1.50 in
ASTM E-8
H.C. Starck 3203 Pure Molybdenum APL, Arc-Cast, Low Carbon Plate
Arc-Cast Plate 3203 Low CarbonDescription of Product: This specification covers rolled plate of carbon-deoxidized molybdenum produced from ingots consolidated by the H.C. Starck consumable electrod..
Tensile Strength >= 517 MPa

@Diameter 3.17 - 10.319 mm
>= 75000 psi

@Diameter 0.125 - 0.40625 in
ASTM E-8
H.C. Starck Pure Molybdenum AB, Arc-Cast Bar
Arc-Cast BarDescription of Product: This specification covers carbon-deoxidized molybdenum wrought bar produced from ingots consolidated by the H.C. Stark consumable electrode vacuum-arc-casting pr..
Tensile Strength >= 517 MPa

@Diameter 28.57 - 47.63 mm
>= 75000 psi

@Diameter 1.125 - 1.875 in
ASTM E-8
H.C. Starck Pure Molybdenum AB, Arc-Cast Bar
Arc-Cast BarDescription of Product: This specification covers carbon-deoxidized molybdenum wrought bar produced from ingots consolidated by the H.C. Stark consumable electrode vacuum-arc-casting pr..
Tensile Strength >= 517 MPa

@Diameter 3.17 - 10.319 mm
>= 75000 psi

@Diameter 0.125 - 0.40625 in
ASTM E-8
H.C. Starck Pure Molybdenum ABL, Arc-Cast, Low Carbon Bar
Description of Product: This specification covers carbon-deoxidized, low-carbon molybdenum wrought bar produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting p..
Tensile Strength >= 517 MPa

@Diameter 28.57 - 47.63 mm
>= 75000 psi

@Diameter 1.125 - 1.875 in
ASTM E-8
H.C. Starck Pure Molybdenum ABL, Arc-Cast, Low Carbon Bar
Description of Product: This specification covers carbon-deoxidized, low-carbon molybdenum wrought bar produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting p..
Tensile Strength 517 - 689 MPa

@Treatment Temp. 1010 - 1090 °C
75000 - 100000 psi

@Treatment Temp. 1850 - 2000 °F
Heat Treatment
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar
Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat..
Tensile Strength 517 - 655 MPa

@Thickness >=25.4 mm
75000 - 95000 psi

@Thickness >=1.00 in
Turned Bars
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar
Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM..