Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 53.0 MPa @Strain 20.0 %, Temperature 23.0 °C |
7690 psi @Strain 20.0 %, Temperature 73.4 °F |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |