Polymer Property : Tensile Strength = 570 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 570 MPa

@Thickness 127 - 152.4 mm
82700 psi

@Thickness 5.00 - 6.000 in
Typical Strength
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength 570 MPa

@Thickness 40.0 - 50.0 mm
82700 psi

@Thickness 1.57 - 1.97 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..