Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 570 MPa @Thickness 127 - 152.4 mm |
82700 psi @Thickness 5.00 - 6.000 in |
Typical Strength |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Tensile Strength | 570 MPa @Thickness 40.0 - 50.0 mm |
82700 psi @Thickness 1.57 - 1.97 in |
Typical Strength |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |