Mechanical Properties Metric English Comments
Tensile Strength >= 758 MPa

@Thickness 12.7 - 25.4 mm
>= 110000 psi

@Thickness 0.500 - 1.00 in
ASTM E-8
H.C. Starck 3403 Molybdenum Alloy APT-3 TZM, Arc-Cast Plate
Arc-Cast Plate 3403Description of Product: This specification covers rolled plate of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated ..
Tensile Strength >= 758 MPa

@Diameter 22.2 - 28.57 mm
>= 110000 psi

@Diameter 0.875 - 1.125 in
ASTM E-8
H.C. Starck Molybdenum Alloy PBT, Bar
Powder Metallurgy BarDescription of Product: This specification covers molybdenum alloy (Molybdenum + 0.5% titanium + 0.1% zirconium) wrought bar produced from pressed and sintered powder metallurg..
Tensile Strength >= 758 MPa

@Diameter 22.2 - 28.57 mm
>= 110000 psi

@Diameter 0.875 - 1.125 in
ASTM E-8
H.C. Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar
Description of Product: This specification covers carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) wrought bar produced from ingots consolidated by the H.C. Starck consuma..
Tensile Strength >= 758 MPa

@Thickness 0.127 - 0.254 mm
>= 110000 psi

@Thickness 0.00500 - 0.0100 in
ASTM E-8
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2
Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req..
Tensile Strength >= 758 MPa

@Thickness 0.254 - 0.508 mm
>= 110000 psi

@Thickness 0.0100 - 0.0200 in
ASTM E-8
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2
Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req..
Tensile Strength >= 758 MPa

@Thickness 0.127 - 0.254 mm
>= 110000 psi

@Thickness 0.00500 - 0.0100 in
ASTM E-8
H.C. Starck 3202 Pure Molybdenum ASL, Arc-Cast, Low Carbon Sheet
Arc-Cast Sheet 3202 Low CarbonDescription of Product: This specification covers rolled sheet of carbon-deoxidized molybdenum produced from sheet bar consolidated by the H.C. Starck consumable elect..
Tensile Strength >= 758 MPa

@Thickness 0.254 - 0.508 mm
>= 110000 psi

@Thickness 0.0100 - 0.0200 in
ASTM E-8
H.C. Starck 3202 Pure Molybdenum ASL, Arc-Cast, Low Carbon Sheet
Arc-Cast Sheet 3202 Low CarbonDescription of Product: This specification covers rolled sheet of carbon-deoxidized molybdenum produced from sheet bar consolidated by the H.C. Starck consumable elect..