Polymer Property : Peel Strength = 0.877 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.526 - 0.877 kN/m

@Temperature -55.0 °C
3.00 - 5.00 pli

@Temperature -67.0 °F
Aluminum, T-Peel
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..