Mechanical Properties Metric English Comments
Peel Strength 0.526 kN/m

@Temperature -55.0 °C
3.00 pli

@Temperature -67.0 °F
180°
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Peel Strength 0.526 - 0.877 kN/m

@Temperature -55.0 °C
3.00 - 5.00 pli

@Temperature -67.0 °F
Aluminum, T-Peel
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Peel Strength 0.526 kN/m

@Temperature 23.0 °C
3.00 pli

@Temperature 73.4 °F
180° T-Peel, Black SBR/CRS
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Peel Strength 0.526 kN/m

@Temperature 175 °C
3.00 pli

@Temperature 347 °F
Adhesion on Aluminum; ASTM D3330
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 0.526 kN/m

@Temperature 175 °C
3.00 pli

@Temperature 347 °F
Adhesion on Aluminum; ASTM D3330
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 0.526 kN/m

@Temperature 175 °C
3.00 pli

@Temperature 347 °F
Adhesion on Aluminum; ASTM D3330
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 0.526 kN/m

@Temperature 175 °C
3.00 pli

@Temperature 347 °F
Adhesion on Aluminum; ASTM D3330
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 0.526 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
3.00 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1870 Industrial Adhesive
Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b..
Peel Strength 0.526 kN/m

@Temperature 49.0 °C
3.00 pli

@Temperature 120 °F
180°
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M
Peel Strength 0.526 kN/m

@Temperature -55.0 °C
3.00 pli

@Temperature -67.0 °F
180°
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M