Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.23 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
7.00 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives
Features: It is a low viscosity grade for spray application.Fast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (Ma..
Peel Strength 1.23 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
7.00 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive
Features: Low viscosity grade for spray applicationFast dryingProvides strong, flexible bondsResists weathering, water, fuels, oil and plasticizersBonds vinyl extrusions and sheeting (May stain ligh..
Peel Strength 1.23 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
7.00 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 5 Neoprene Contact Adhesive
3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInforma..
Peel Strength 1.23 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
7.00 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 4475 Industrial Adhesive
Features: Dries quickly to a firm bondExcellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greasesA general purpose adhesive for bonding most vinyls, cer..
Peel Strength 1.23 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
7.00 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives
Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a..
Peel Strength 1.23 kN/m

@Temperature 24.0 °C,
Time 259000 sec
7.00 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1870 Industrial Adhesive
Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b..
Peel Strength 1.23 kN/m

@Temperature 24.0 °C,
Time 432000 sec
7.00 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1870 Industrial Adhesive
Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b..
Peel Strength 1.23 kN/m

@Temperature 24.0 °C,
Time 605000 sec
7.00 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1870 Industrial Adhesive
Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b..
Peel Strength 1.23 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
7.00 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1870 Industrial Adhesive
Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b..
Peel Strength 1.23 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
7.00 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1870 Industrial Adhesive
Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b..