Material Notes:
Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (May stain light colored vinyls.)Also bonds fabrics, foams and many plastics. (Not recommended for polyolefin plastic bonding)May be heat cured to obtain superior physical propertiesInformation provided by 3M
Physical Properties Metric English Comments
Solids Content 31 - 37 %
31 - 37 %
Brookfield Viscosity 2000 - 4000 cP
2000 - 4000 cP
RVF #3 sp @ 10 rpm
Mechanical Properties Metric English Comments
Shear Strength 3.22 MPa

@Temperature 121 °C
467 psi

@Temperature 250 °F
Overlap, 1/8" Alum/Alum
4.19 MPa

@Temperature 93.0 °C
607 psi

@Temperature 199 °F
Overlap, 1/8" Alum/Alum
4.43 MPa

@Temperature 82.0 °C
643 psi

@Temperature 180 °F
Overlap, 1/8" Alum/Alum
6.18 MPa

@Temperature 65.0 °C
897 psi

@Temperature 149 °F
Overlap, 1/8" Alum/Alum
9.005 MPa

@Temperature 24.0 °C
1306 psi

@Temperature 75.2 °F
Overlap, 1/8" Alum/Alum
20.61 MPa

@Temperature -55.0 °C
2989 psi

@Temperature -67.0 °F
Overlap, 1/8" Alum/Alum
23.50 MPa

@Temperature -34.0 °C
3409 psi

@Temperature -29.2 °F
Overlap, 1/8" Alum/Alum
Peel Strength 0.614 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
3.50 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
1.23 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
7.00 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
2.89 kN/m

@Temperature 24.0 °C,
Time 86400 sec
16.5 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
3.07 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
17.5 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
4.12 kN/m

@Temperature 24.0 °C,
Time 432000 sec
23.5 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
4.56 kN/m

@Temperature 24.0 °C,
Time 259000 sec
26.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
4.82 kN/m

@Temperature 24.0 °C,
Time 605000 sec
27.5 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
5.26 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
5.43 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
31.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
Thermal Properties Metric English Comments
Flash Point -18.0 °C
-0.400 °F
TCC
Descriptive Properties Value Comments
Appearance Light tan
Base Nitrile Rubber