Polymer Property : Peel Strength = 123 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 19.6 - 21.6 kN/m

@Temperature 99.0 °C
112 - 123 pli

@Temperature 210 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers