Polymer Property : Peel Strength = 138 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 24.2 kN/m

@Temperature 90.5 °C
138 pli

@Temperature 195 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 429 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Peel Strength 24.2 kN/m

@Temperature 99.0 °C
138 pli

@Temperature 210 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 429 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers