Polymer Property : Peel Strength = 17.5 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 3.07 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
17.5 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives
Features: It is a low viscosity grade for spray application.Fast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (Ma..
Peel Strength 3.07 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
17.5 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive
Features: Low viscosity grade for spray applicationFast dryingProvides strong, flexible bondsResists weathering, water, fuels, oil and plasticizersBonds vinyl extrusions and sheeting (May stain ligh..
Peel Strength 3.07 kN/m

@Temperature -34.0 °C
17.5 pli

@Temperature -29.2 °F
180°, Canvas/Steel
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov..
Peel Strength 3.07 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
17.5 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives
Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a..