Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 5.65 kN/m @Temperature -54.0 °C |
32.2 pli @Temperature -65.2 °F |
Metal-to-metal |
Hexcel® HexPly® F185 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F185; Fiber: 75-1/0Information provided by HexCel |