Mechanical Properties Metric English Comments
Peel Strength 5.65 kN/m

@Temperature -54.0 °C
32.2 pli

@Temperature -65.2 °F
Metal-to-metal
Hexcel® HexPly® F185 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F185; Fiber: 75-1/0Information provided by HexCel