Polymer Property : Peel Strength = 43.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 7.54 kN/m

@Temperature 121 °C
43.0 pli

@Temperature 250 °F
Roller Peel, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D3167
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive
Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive character..