Mechanical Properties Metric English Comments
Ball Indentation Hardness 150 MPa

@Load 36.5 kg
21800 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Ball Indentation Hardness 150 MPa

@Load 36.5 kg
21800 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced
Flame retarded (class V0), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th..
Ball Indentation Hardness 150 MPa

@Load 36.5 kg
21800 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced
Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th..
Ball Indentation Hardness 150 MPa

@Load 36.5 kg
21800 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Ball Indentation Hardness 150 MPa

@Load 36.5 kg
21800 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced
Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has ..
Ball Indentation Hardness 150 MPa

@Load 36.5 kg
21800 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MCS Polyamide 6 - Colored
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For colored parts produced by injection molding.Tarnamid® has the following ..
Ball Indentation Hardness 150 MPa

@Load 36.5 kg
21800 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored
Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper..
Ball Indentation Hardness 150 MPa

@Load 36.5 kg
21800 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored
High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration..