Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 94.0 MPa @# of Cycles 1.00e+7 |
13600 psi @# of Cycles 1.00e+7 |
R.R. Moore Test, Smooth Rotating Beam |
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |