Polymer Property : Fatigue Strength = 94.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 94.0 MPa

@# of Cycles 1.00e+7
13600 psi

@# of Cycles 1.00e+7
R.R. Moore Test, Smooth Rotating Beam
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..