Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 240 - 270 MPa @# of Cycles 1.00e+8 |
34800 - 39200 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl.. |
|||
Fatigue Strength | >= 240 MPa @# of Cycles 1.00e+7 |
>= 34800 psi @# of Cycles 1.00e+7 |
(R=-1) |
Schmolz + Bickenbach MoldMAX® SC Copper Alloy Description: Brush Wellman’s MoldMAX® SC is a high conductivity copper mold alloy with good strength. MoldMAX® SC is used as blow mold cavities, injection mold cores and cavities and hot .. |
|||
Fatigue Strength | 240 MPa | 34800 psi | rotational bending |
CLAL-MSX CUPROROR® TL5 Spring, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Fatigue Strength | >= 240 MPa @# of Cycles 1.00e+7 |
>= 34800 psi @# of Cycles 1.00e+7 |
(R=-1) |
Schmolz + Bickenbach MoldMAX XL® Copper Alloy Description: Brush Wellman’s MoldMAX XL® is a high strength copper mold alloy with good thermal conductivity. The alloy contains no beryllium and is available in sections as large as 12” thick. .. |